Making a thin section
A thin section is a slice of rock ground so thin, 30 micrometres or 0.03 millimetres, that light passes straight through most minerals. Under a polarising microscope each mineral then shows its own colours and shapes, and a meteorite that looks grey to the eye turns into a mosaic of chondrules, crystals and metal. Almost every new meteorite is classified from a thin section, and the method has hardly changed in principle since the 1850s: a flat face, glue, glass and patient grinding.
Laboratory safety
- Making thin sections is adult work, normally done in a laboratory with proper training. Students learn most by looking at finished sections.
- Uncured epoxy resin and hardener can cause skin allergies that last for life. Wear nitrile gloves and eye protection, mix resin in a ventilated place and never let it touch your skin.
- Hot plates used to cure resin reach temperatures that burn. Keep them clear of solvents and paper, and let them cool before you touch the slide.
- Grinding produces fine rock and metal dust in the slurry. Keep it wet, wipe up spills rather than letting them dry, and do not breathe dust from dried residues.
- Acetone and alcohol used for cleaning slides are highly flammable: keep them capped, labelled and away from flames and hot plates.
- Saws used to trim the chip have the same dangers as any diamond saw: guards on, eye protection, and the chip held in a chuck, never in your fingers.
Before you start: Never cut, grind, etch, heat or clean with liquids a stone that has not been confirmed as a meteorite by a museum, a university or a recognised laboratory. Read Before you start: what not to do first.
Making thin sections needs laboratory equipment: a precision saw, a vacuum impregnation unit, a lapping machine, a hot plate and a polarising microscope. Most collectors, schools and clubs have sections made by a specialist preparation laboratory, and spend their time looking at them.
-
Step 1: Choose and cut the chip
A thin section starts as a small block called a chip or billet, cut from an end piece or the edge of a slice with a precision saw. It must fit the glass slide, so it is usually no larger than about 20 by 40 mm, and a few millimetres thick. The scientist chooses the place carefully: an area that shows the typical texture of the meteorite, or a particular feature such as a large chondrule, a dark clast or a shock vein. The position of the chip is marked on a photograph or a sketch of the parent piece.
For a meteorite that is very small or very precious, a few loose fragments can be set in resin instead, making a grain mount.
Why it matters: The section shows only a few square centimetres of a rock that may weigh kilograms, so where it comes from decides what it can tell you. Recording the position lets a later researcher go back to the same part of the meteorite.
For this step
- Low-speed precision saw or a thin-bladed trim saw
- Water-free coolant or oil for metal-rich and salt-bearing stones
- Callipers
- Photograph or sketch of the parent piece for marking the chip's position
- Labels and a sample register
Common mistakes
- Taking the chip from a weathered rim instead of the fresh interior
- Cutting a chip larger than the slide, so it must be trimmed again
- Forgetting to record where in the meteorite the chip came from
- Cutting a salt-bearing or rust-prone meteorite with water
Laboratory or collector? In research the chip is chosen to answer a question and its position is logged in a collection database. Collectors who buy ready-made sections should still ask which meteorite and which piece each one came from: a section without that record is just a pretty picture.
-
Step 2: Fill the pores with resin
Many meteorites are crumbly or full of tiny cracks: carbonaceous chondrites, weathered desert finds, breccias and shocked stones. Before they can be ground thin, the chip is impregnated: it is placed in a dish of low-viscosity epoxy resin inside a vacuum chamber. The vacuum draws the air out of the pores, and when air is let back in, its pressure pushes resin deep into every crack. The resin is then cured, often on a warm plate, until it is hard.
Why it matters: At 30 micrometres a rock has almost no strength. Without resin in its pores, loose chondrules and crystals are torn out during grinding and leave holes, and the section can break apart completely.
For this step
- Low-viscosity epoxy resin and hardener made for thin sections
- Vacuum chamber or vacuum impregnation unit
- Disposable mixing cups and stirrers
- Hot plate or curing oven
- Nitrile gloves, eye protection and good ventilation
Common mistakes
- Skipping impregnation on a friable stone
- Mixing resin and hardener in the wrong ratio, so it never fully hardens
- Stirring in air bubbles, which become holes in the section
- Heating too fast, so the resin boils or the chip cracks
Laboratory or collector? Laboratories impregnate almost every fragile sample as routine, and record the resin used, because it contains carbon that could confuse chemical analyses. Some laboratories avoid resin altogether for samples meant for organic chemistry.
-
Step 3: Grind one face perfectly flat
One face of the chip is ground flat and smooth, because this is the face that will be glued to the glass. It is worked on a rotating lap or by hand on a thick glass plate with silicon carbide grit and a little liquid, from coarse to fine: for example about 220 grit, then 600, then 1000. The chip is cleaned thoroughly between grits so that no coarse grains are carried on to the finer stage. The finished face is dull but even and completely flat.
Why it matters: Any hollow in this face becomes a pocket of glue or air between rock and glass. When the section is later ground to 30 micrometres, those areas grind away or come loose, and the section ends up with holes or patches of the wrong thickness.
For this step
- Rotating lap or a thick glass grinding plate
- Silicon carbide grit, coarse to fine (about 220, 600 and 1000)
- Oil or alcohol instead of water for rust-prone or salt-bearing meteorites
- Lint-free cloths and an ultrasonic cleaner
Common mistakes
- Rocking the chip while grinding, so the face becomes rounded
- Carrying coarse grit on to a finer stage, which leaves deep scratches
- Leaving the face wet or oily before gluing, so the bond fails
- Grinding an iron-rich chip with water and leaving it to dry slowly
Laboratory or collector? Both laboratories and amateur section makers work this stage the same way. Laboratories often use machines that hold the chip square to the lap, while hobbyists rely on a flat glass plate and a steady hand.
-
Step 4: Bond the chip to the glass slide
A glass slide is frosted on one side by grinding it lightly with fine grit, so that the glue grips. A thin layer of epoxy is spread on the slide, and the flat face of the chip is lowered on to it at an angle to push the air out. The chip is pressed down evenly, often in a small clamp or jig, and the epoxy is cured. Slides are commonly about 27 by 46 mm, or the standard 26 by 76 mm microscope size. In the past the glue was Canada balsam, a natural tree resin; epoxies with almost the same optical properties replaced it because they are stronger and do not soften with warmth.
Why it matters: The glue must be thin, even and free of bubbles, and it must hold every grain when the rock is no thicker than a hair. Its clarity matters too: the light that shows the minerals passes through it.
For this step
- Glass slides, frosted on one side
- Thin-section epoxy
- Bonding jig or light clamp
- Hot plate for curing
- Diamond scribe to engrave the sample number on the glass
Common mistakes
- Trapping air bubbles under the chip
- Using too much glue, so the layer is thick and uneven
- Pressing harder on one side, so the chip sits at a slope
- Labelling the slide with ink that dissolves in the cleaning solvents
Laboratory or collector? Laboratories engrave a sample number into every slide with a diamond scribe before anything else, because a numbered slide can never be confused with another. That habit is worth copying by anyone who makes sections.
-
Step 5: Cut off the chip and grind down
Most of the chip is now sliced away with a precision saw, leaving a layer about half a millimetre to a millimetre thick on the glass. This is then ground thinner, first quickly on a coarse diamond wheel or lap to about 100 micrometres, then slowly with fine silicon carbide or diamond abrasives. Near the end, a few seconds of grinding can remove 10 micrometres, so the slide is checked under the microscope again and again. Thickness can also be measured with a micrometer as the total thickness of slide and section, minus the glass.
Why it matters: Grinding fast to near the target saves hours; grinding slowly at the end saves the section. Once a mineral is ground too thin, it cannot be put back.
For this step
- Precision saw with a slide holder
- Diamond grinding wheel or lap for the coarse stage
- Fine silicon carbide or diamond abrasives for the last stage
- Micrometer
- Polarising microscope beside the bench
Common mistakes
- Grinding coarse right down to the target, so the section is torn and scratched
- Pressing unevenly, so one end is thinner than the other
- Not checking often enough near the end
- Letting the slide overheat on a machine, which softens the glue
Laboratory or collector? Laboratories use thin-section machines that hold the slide on a vacuum chuck and grind it to a set thickness. Hobbyists can make good sections by hand on glass plates, but it takes practice and many spoiled slides.
-
Step 6: Check the thickness by the colours
A polarising microscope has two polarising filters set at right angles, called crossed polars. Between them, most minerals show interference colours, and those colours depend on two things: the mineral's birefringence (how strongly it splits light) and the thickness of the section. So a mineral of known birefringence acts as a gauge. In ordinary rocks, quartz is used: at 30 micrometres it shows pale grey and white. Meteorites rarely contain quartz, so section makers watch other minerals: olivine should show bright second- and third-order blues, greens, pinks and yellows, and feldspar should show first-order greys. If the colours are higher than they should be, the section is still too thick.
Why it matters: Mineral identification depends on comparing the colours you see with the colours a mineral shows at standard thickness. A section that is too thick gives colours that are too high and makes minerals hard to tell apart; one that is too thin makes everything look grey and starts to lose grains.
For this step
- Polarising microscope with crossed polars
- An interference colour chart
- Fine abrasive and a glass plate for the last few micrometres
- Notebook to record the final thickness
Common mistakes
- Judging thickness by eye instead of by the colours
- Using a mineral of unknown composition as the gauge
- Forgetting that the edge of a section often grinds thinner than the middle
- Going on grinding after the colours are right, just to be sure
Laboratory or collector? This test is the same in every laboratory and classroom. Many research sections of meteorites are deliberately made a little thinner or thicker for special purposes, and the thickness is then written on the label.
-
Step 7: Polish or cover, then label
A section made for teaching is often finished with a thin glass cover slip glued on top. Most meteorite sections are instead left uncovered and polished with diamond paste, working down through about 6, 3 and 1 micrometre, sometimes to 0.25. A polished section can be studied in two ways at once: in light passing through it, for the silicate minerals, and in light reflected from its surface, for the opaque metal, sulphides and oxides. Coated with a very thin layer of carbon, the same slide can then go into an electron microprobe or a scanning electron microscope to measure the chemistry of single grains.
The slide is cleaned, its number and the meteorite's name are written on a label, and it is stored flat in a slide box, away from damp.
Why it matters: Polishing turns one section into a sample for three instruments, so a tiny amount of precious meteorite answers many questions. In iron-bearing meteorites the polished metal can rust, so these slides need dry storage like any other specimen.
For this step
- Diamond pastes or suspensions, about 6, 3, 1 and 0.25 micrometres
- Polishing cloths on a lap
- Cover slips and mounting medium (for covered sections)
- Carbon coater (in laboratories)
- Slide boxes and archival labels
Common mistakes
- Covering a section that later needs microprobe work, since a cover slip blocks the beam
- Using a single polishing cloth for every grade, so coarse diamond scratches the final surface
- Polishing with water-based liquids on rust-prone meteorites
- Storing polished slides in damp rooms, where the metal grains rust
Laboratory or collector? Scientists almost always want polished, uncovered sections because they can go straight to the microprobe. Collectors often buy covered sections, which are tougher and look beautiful under a simple polarising microscope.
Why 30 micrometres?
At this thickness most rock-forming minerals let light through, and each shows interference colours low enough to identify. Thicker, and the colours become washed-out pastel pinks and greens that are hard to tell apart; thinner, and many minerals fade to grey. The value became a worldwide standard so that every geologist's colour charts would match.
What a thin section shows in a meteorite
In a chondrite you see round chondrules with their crystals of olivine and pyroxene, a fine-grained matrix between them, and opaque grains of metal and troilite that stay black in transmitted light. In achondrites you see interlocking crystals like those of volcanic rocks on Earth. The texture, the minerals and the signs of shock and heating are enough to give most meteorites a preliminary class.
Choose a chip that represents the meteorite and record where it came from, fill its pores with resin, grind one face perfectly flat, bond it to frosted glass without bubbles, saw and grind it down slowly, use the interference colours of known minerals to stop at 30 micrometres, then polish or cover it and label it.
Related pages
- How do scientists cut and study a meteorite?
- How can I use microscopes to study meteorites in class?
- What is a chondrule?
- What is the matrix of a chondrite?
Glossary: Thin section, Polarising microscope, Electron microprobe, Scanning electron microscope, Olivine, Pyroxene, Plagioclase, Chondrule, Matrix