Meteorite types: Advanced course · Lesson 5 of 6

Crystallising iron cores

A magmatic iron group is a series of snapshots of one core freezing. Trace elements that prefer the solid or the liquid change in predictable ways as crystallisation proceeds, and the metal's microstructure records how fast that core lost its heat.

In this lesson you will
  • Use partition coefficients to explain why some elements fall and others rise through a magmatic iron group.
  • Apply the Rayleigh fractional crystallisation equation to model trace element trends.
  • Interpret metallographic cooling rates and low-temperature microstructures in terms of parent body history.

Links to: A-level chemistry: transition metals and equilibrium; A-level geology: fractional crystallisation; A-level maths: exponents, logarithms and modelling.

Partition coefficients

When a liquid metal core cools, solid metal crystallises from it. Each element divides itself between the solid and the remaining liquid according to its partition coefficient, D = concentration in solid ÷ concentration in liquid.

Elements with D > 1 are compatible: they enter the solid preferentially. Iridium, osmium and rhenium are strongly compatible. Elements with D < 1 are incompatible: they build up in the liquid. Gold, arsenic and phosphorus are examples, and nickel is slightly incompatible. Sulfur is almost completely excluded from solid metal, so it accumulates in the liquid as crystallisation goes on, and rising sulfur makes compatible elements even more compatible.

Rayleigh fractionation and group trends

If each crystal is removed from contact with the liquid as it forms, the composition of the solid follows the Rayleigh equation:

C_solid = D × C₀ × (1 − F)^(D − 1),

where C₀ is the starting concentration in the liquid and F is the fraction already crystallised. For D > 1 the solid gets steadily poorer in the element; for D < 1 it gets richer.

This is exactly what magmatic groups show. Through the IIIAB irons, iridium falls by a factor of about a thousand while nickel rises only from roughly 7 to 10% and gold increases. On a log–log plot of iridium against gold, the members of a magmatic group lie on a single curved trend, which is the strongest evidence that each group is one core. The IAB irons scatter instead, consistent with their formation in separate impact-melt pools rather than in one fractionating core.

Metallographic cooling rates

Below about 700–500 °C, depending on nickel content, kamacite grows from taenite. Nickel diffuses through the metal so slowly that the taenite is left with an M-shaped nickel profile, richer at its edges than at its centre. Computer models of diffusion turn the shape of that profile into a cooling rate.

If a core cooled inside an insulating mantle, all its parts should have cooled at about the same rate. IIIAB irons broadly fit this, at roughly 50–350 °C per million years. The IVA irons do not: their cooling rates range from about 100 to several thousand °C per million years and vary with nickel content. That suggests a metal body that crystallised and cooled with little or no rocky mantle around it, perhaps after a collision stripped the mantle away. Some metal-rich asteroids, such as Psyche, may be cores exposed in this way.

Records below 400 °C

As the metal cools further, new structures form. Below about 320 °C, nickel-rich taenite can order into tetrataenite, and next to it forms the cloudy zone, a fine intergrowth of tetrataenite islands in a nickel-poorer matrix. The size of the islands is another cooling-rate indicator, sensitive to much lower temperatures.

Tetrataenite is also an excellent magnetic recorder. Magnetic measurements of cloudy zones in some pallasites and irons suggest that their parent bodies' cores generated a magnetic field, a dynamo, while they were crystallising, just as Earth's core does today. Iron meteorites thus give evidence about core convection on bodies only a few hundred kilometres across. Combined with hafnium–tungsten ages showing that many cores separated within 1–2 million years of CAIs, they make iron meteorites the most detailed record of planetary cores in existence.

Worked example

Modelling iridium and gold in a crystallising core

A core liquid starts with C₀ = 1 (in arbitrary units) of both iridium (D = 4) and gold (D = 0.3). Use C_solid = D × C₀ × (1 − F)^(D − 1) to find the concentration in the solid when F = 0 and F = 0.8.

  1. Iridium, F = 0: C = 4 × 1 × 1³ = 4.
  2. Iridium, F = 0.8: C = 4 × 0.2³ = 4 × 0.008 = 0.032, a fall by a factor of 125.
  3. Gold, F = 0: C = 0.3 × 1 × 1⁻⁰·⁷ = 0.3.
  4. Gold, F = 0.8: C = 0.3 × 0.2⁻⁰·⁷ ≈ 0.3 × 3.09 ≈ 0.93, a rise by a factor of about 3.

Answer: Iridium falls steeply and gold rises gently, the pattern seen across magmatic groups such as IIIAB. Rising sulfur in the liquid would make the iridium fall even steeper.

Activity

Using the Rayleigh equation, calculate the solid concentration of an element with D = 2 and of one with D = 0.5 at F = 0, 0.2, 0.4, 0.6 and 0.8, with C₀ = 1. Plot both on the same graph against F and describe how the shapes differ. Then explain what a scattered, trendless group, like IAB, would tell you instead.

Quiz

15 questions, picked at random from a bank of 30, so every try is different. Score 12 or more to pass. Choose an answer to see whether you are right and why.

  1. Question 1What does a partition coefficient D measure?

  2. Question 2Which element is strongly compatible in solid iron metal?

  3. Question 3An element with D = 0.2 is described as what?

  4. Question 4Why does sulfur build up in the remaining core liquid?

  5. Question 5How does rising sulfur in the liquid affect iridium?

  6. Question 6In the Rayleigh equation, what does F stand for?

  7. Question 7For an element with D > 1, what happens to its concentration in new solid as F rises?

  8. Question 8Through the IIIAB irons, roughly how much does iridium change?

  9. Question 9How does nickel change across the IIIAB irons?

  10. Question 10What is the strongest evidence that a magmatic group comes from one core?

  11. Question 11Why do IAB irons scatter on element plots?

  12. Question 12With D = 3 and C₀ = 1, what is C_solid at F = 0.5?

  13. Question 13With D = 1, what happens to C_solid as crystallisation proceeds?

  14. Question 14In the worked example, why does gold rise only gently while iridium falls steeply?

  15. Question 15What shape does the nickel profile across a taenite grain usually have?

  16. Question 16How is a metallographic cooling rate obtained?

  17. Question 17What would you expect if a core cooled inside a thick insulating mantle?

  18. Question 18What do the widely varying IVA cooling rates suggest?

  19. Question 19Roughly what cooling rates do IIIAB irons record?

  20. Question 20A core cools at 100 °C per million years from 700 °C to 400 °C. How long does this take?

  21. Question 21Why might the asteroid Psyche be important for iron meteorite studies?

  22. Question 22Below about what temperature does tetrataenite form?

  23. Question 23What is the cloudy zone?

  24. Question 24What do cloudy-zone magnetic records suggest about some parent bodies?

  25. Question 25Why is tetrataenite a good magnetic recorder?

  26. Question 26What do hafnium–tungsten ages show about iron meteorite cores?

  27. Question 27Why is the cloudy zone useful in addition to Widmanstätten-based cooling rates?

  28. Question 28An element shows no trend and wide scatter across a group. Which interpretation fits best?

  29. Question 29Two irons from one magmatic group have very different iridium. Which crystallised earlier?

  30. Question 30Which element should increase in the solid as a core crystallises?

Explore on Howardites